We would not recommend PERMASET Inks. PERMAPRINT Premium Inks have been tested on clear vinyl film with good results. However, there is a risk that the ink will soften over time if there’s plasticiser migration from the vinyl film. This can be reduced by wiping the film down with acetone prior to printing, but this only forestalls the inevitable. The plasticiser will eventually migrate out of the film and into the ink. Thus this system may be viable for shorter term and low/no abrasion applications, it is not recommended for long term high abrasion installations.